粘土磚及高鋁磚 |
|
 |
|
高鋁磚
|
一級高鋁 |
二級高鋁 |
三級高鋁 |
LZ-75 |
LZ-65 |
LZ-55 |
LZ-48 |
Al2O3,≥ % |
75 |
65 |
55 |
48 |
耐火度 Refractoriness,≥,℃ |
1790 |
1770 |
1750 |
0.2Mpa 荷重軟化開始溫度 RUL, T0.6,℃≥,℃ |
1520 |
1500 |
1470 |
1420 |
重燒線變化 Linear change on reheating,% |
1500℃×2h |
+0.1 |
-0.4 |
-0.4 |
1450℃×2h |
— |
— |
+0.1 -0.4 |
顯氣孔率 Apparent porosity,≤ % |
23 |
22 |
常溫耐壓強度 CCS,≥Mpa |
≥53.9 |
≥49.0 |
≥44 |
≥40 |
粘土磚
|
NZ-45 |
NZ-40 |
Al2O3,%,≥ |
45 |
40 |
耐火度 Refractoriness,℃ |
1750 |
1730 |
荷重軟化溫度 RUL,T0.6,℃ |
1400 |
1350 |
重燒線變化 Linear change on reheating(1400 ℃×2h),% |
-0.4~+0.1 |
-0.5~+0.1 |
顯氣孔率 Apparent porosity,% |
22 |
24 |
耐壓強度 CCS,Mpa |
30 |
25 |
熱震穩定性 Thermal shock resistance |
良好 Excellent |
|
|
|
|
|